Tensile Strength, Ultimate 538 MPa

@Temperature 316 °C
78000 psi

@Temperature 601 °F
Haynes Multimet® alloy, sand cast, 1171°C heat treatment for 2 hours
Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit..
Tensile Strength, Ultimate 538 MPa
78000 psi
Kinetics MIM 316 Stainless Steel (Premium Grade)
Austenitic stainless steel. Excellent corrosion resistance. Excellent elongation. Non-magnetic. Easily weldable. Can be polished to a mirror finish. Provides better elongation and ductility over the..
Tensile Strength, Ultimate 538 MPa
78000 psi
Kinetics MIM 316 Stainless Steel (Standard Grade)
Austenitic stainless steel. Excellent corrosion resistance. Non-magnetic. Lower cost, elongation, and ductility than “premium” grade. Often used for food industry, marine, medical, and app..
Tensile Strength, Ultimate 538 MPa
78000 psi
Universal Wire Works 330 Stainless Steel Electrode
Universal 330 electrodes are used to weld cast and wrought forms of type 330 stainless steel. The high nickel content of this electrode provides excellent resistance to heat and scale at temperature..
Tensile Strength, Ultimate 538 MPa
78000 psi
Universal Wire Works 430 Stainless Steel Electrode
Universal 430 electrode deposits contain approximately 16% chromium in a carefully balanced composition to provide outstanding resistance at temperatures up to 1600 degrees F. Deposits are martensit..
Tensile Strength, Ultimate 538 - 627 MPa
78000 - 91000 psi
Eagle Brass 18665 MSP1, Extra Hard
MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs..
Tensile Strength, Ultimate 538 - 593 MPa
78000 - 86000 psi
Eagle Brass 230 Red Brass, Spring
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Ultimate 538 - 600 MPa
78000 - 87000 psi
Eagle Brass 240 Low Brass, Extra Hard
CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib..
Tensile Strength, Ultimate 538 - 641 MPa
78000 - 93000 psi
Eagle Brass 519 Phosphor Bronzes 6%, Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
Tensile Strength, Ultimate 538 - 607 MPa
78000 - 88000 psi
Eagle Brass 706 Copper Nickel 10%, Spring
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Tensile Strength, Ultimate 538 - 627 MPa
78000 - 91000 psi
Eagle Brass 752 Nickel Silver 18%, Hard
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..
Tensile Strength, Ultimate 538 - 655 MPa
78000 - 95000 psi
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Tensile Strength, Ultimate 538 MPa
78000 psi
annealed
CMW® ELKONIUM 43 palladium based alloy
Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi..
Tensile Strength, Ultimate 538 MPa
78000 psi
AK Steel 18 SR® Ferritic Stainless steel
AK Steel 18 SR® provides excellent resistance to high temperature scaling - far superior to that of Type 446 stainless steel. This material is readily welded by conventional methods. It is not su..
Tensile Strength, Ultimate 538 MPa

@Temperature 566 °C
78000 psi

@Temperature 1050 °F
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Ultimate 538 MPa
78000 psi
Transverse, Welded
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406
Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat..
Tensile Strength, Ultimate 538 MPa
78000 psi
Typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410HC
Allegheny Ludlum Type 410HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl..