Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 510 MPa

@Temperature 400 °C
74000 psi

@Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..
Tensile Strength, Ultimate 510 MPa
74000 psi
Kinetics MIM K1 Kinetics Custom Alloy
K1 is a custom alloy that provides very high wear resistance. Possible applications include agricultural implements, high security lock components, and wear surface applications in assemblies. This ..
Tensile Strength, Ultimate 510 - 610 MPa
74000 - 88500 psi
Materion Beryllium Copper Alloy 25 Strip; 1/4 H (TD01) Temper (UNS C17200)
Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 62-75Tabulated properties apply ..
Tensile Strength, Ultimate 510 MPa

@Temperature 870 °C
74000 psi

@Temperature 1600 °F
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 510 - 725 MPa
74000 - 105000 psi
Materion Brush 1915â„¢ Heat Treated Temper Wire, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Tensile Strength, Ultimate 510 MPa

@Temperature 650 °C
74000 psi

@Temperature 1200 °F
Haynes 25 alloy, vacuum investment castings, solution treated
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 510 MPa

@Temperature 538 °C
74000 psi

@Temperature 1000 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Ultimate 510 MPa
74000 psi
Superior Die Set FORTAL® HP Aluminum Alloy
Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and d..
Tensile Strength, Ultimate 510 MPa
74000 psi
Wieland 1744 Wilaform Platinum
Hard platinum alloy for strongly stressed decorationApplications: chains, laminar decoration, pipes, tubingDental
Tensile Strength, Ultimate 510 - 593 MPa
74000 - 86000 psi
Eagle Brass 752 Nickel Silver 18%, 3/4 Hard
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..
Tensile Strength, Ultimate 510 MPa

@Temperature 371 °C
74000 psi

@Temperature 700 °F
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..
Tensile Strength, Ultimate 510 MPa
74000 psi
Annealed
ATI Allegheny Ludlum 410 Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Tensile Strength, Ultimate 510 - 550 MPa
74000 - 79800 psi
L direction
ArcelorMittal Save 20-15 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 510 - 550 MPa
74000 - 79800 psi
L direction
ArcelorMittal Save 25-16 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 510 - 550 MPa
74000 - 79800 psi
L direction
ArcelorMittal Save 27-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 510 - 550 MPa
74000 - 79800 psi
L direction
ArcelorMittal Save 30-17 Electrical Steel
Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..
Tensile Strength, Ultimate 510 MPa
74000 psi
Typical
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel
Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab..