Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 450 MPa @Temperature 100 °C |
65300 psi @Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
MetalTek C86500 Low Tensile Manganese Bronze High aqueous and atmospheric corrosion resistance, moderate strength and conductivity.Applications: Valves, pumps, pipe fittings, electric terminal ends.Information provided by MetalTekCast UNS C836.. |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
MetalTek MTEK 125 Cast UNS C95200 Aluminum Bronze Versatile alloy with high strength, good ductility, unusual toughness, plus exceptional wear resistance. Aluminum Bronze heat treated to higher mechanical properties where necessary.Information prov.. |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
MetalTek MTEK 25-20 Cast UNS J94224 Heat Resistant Stainless Steel Increased strength for more highly stressed applications. Good resistance to oxidizing or reducing process flow.Applications: Calcining tubes, pier caps, high temperature fixtures and hardware.Infor.. |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
MetalTek MTEK 25-35Nb Heat Resistant Stainless Steel Information provided by MetalTekCast ASTM A297 MOD. |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
MetalTek MTEK 28-48WCo Heat Resistant Stainless Steel Information provided by MetalTek |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
MetalTek MTEK 30-20 Cast UNS N08604 Heat Resistant Stainless Steel Provides strength levels of HK with improved corrosion resistance to hot gases.Applications: Similar to HN.Information provided by MetalTekCast UNS N08604; Cast Grade HL; Cast ASTM A297, A608 |
|||
Tensile Strength, Ultimate | 450 - 550 MPa | 65300 - 79800 psi | |
CLAL-MSX ARCAP Anticorrosion AP1 H12 1/2 hard, Rolled Copper Alloy Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (accordin.. |
|||
Tensile Strength, Ultimate | <= 450 MPa | <= 65300 psi | Rod |
CLAL-MSX ARCAP Anticorrosion AP1C 0 Annealed, Drawn Copper Alloy Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un.. |
|||
Tensile Strength, Ultimate | 450 MPa | 65300 psi | As Cast |
AFE Technologies Cronite 657 Nickel Alloy Castings High temperature nickel alloy castings. Applications include heat treatment and handling products, furnace products, tubes, power generation, and petrochemical industries.Information provided by AF.. |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
AK Steel ASTM A 1011, Class 1 Formable, Grade 50K Hot Rolled Carbon Steel, Medium/High Strength Low Alloy Steel (HSLA) Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
AK Steel ASTM A 570, Grade 50 Hot Rolled Carbon Steel, Structural Quality (SQ) For gauges up to 0.229", ASTM A 570 must be specified, gauges >0.230", ASTM A 907 must be used. Items 0.180 to 0.230" gauge which are >48" wide may be ordered to either A 570 or A 907.Information p.. |
|||
Tensile Strength, Ultimate | 450 MPa | 65300 psi | |
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel DI-MAX HF-10 is a fully processed nonoriented electrical steel designed for use in high speed motors, traction motors, aircraft generators, and other rotating equipment operating at frequencies abov.. |
|||
Tensile Strength, Ultimate | 450 - 530 MPa | 65300 - 76900 psi | |
ArcelorMittal Dual Phase 450 Very high strength steel, Cold Rolled Steel Available in the following: HCT500X (uncoated), HCT500X+ZE (electrogalvanized) and HCT500X+Z (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength and .. |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | Minimum Guaranteed |
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |
|||
Tensile Strength, Ultimate | >= 450 MPa | >= 65300 psi | |
MetalTek MTEK A Cast UNS N04020 Nickel-Copper Alloy Acid and alkaline resistant. Weldable gradeApplications: Marine pumps, valves, seal housings, filter parts.Information provided by MetalTek |