Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 41.2 MPa @Temperature 260 °C |
5980 psi @Temperature 500 °F |
ASTM D-638 |
UBE UPIMOL® R Polyimide Shape Description: Ube's UPIMOL is an exceptionally heat-resistant polyimide Shape. This product has the same molecular structure as UPILEX, an ultra-high heat-resistant polyimide film developed by Ub.. |
|||
Tensile Strength, Ultimate | 41.2 MPa @Temperature 260 °C |
5980 psi @Temperature 500 °F |
ASTM D1708 |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Tensile Strength, Ultimate | 41.2 MPa @Temperature 260 °C |
5980 psi @Temperature 500 °F |
ASTM D1708 |
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS .. |
|||
Tensile Strength, Ultimate | 41.2 MPa | 5980 psi | ASTM D638 |
BCC Products BC 8086 Urethane Casting BC 8086 is a rapid setting, low viscosity, polyurethane casting system. It exhibits a working life of 45 seconds and obtains a demoldable hardness at 7 - 10 minutes. Some of the features include: no.. |