Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3.79 - 4.48 MPa | 550 - 650 psi | |
Sika Industry SikaFlex 252 One Part Polyurethane Adhesive Sika 252 SikaFlex One Part Polyurethane AdhesiveA high viscous, high strength adhesive, this product can replace rivets, screws, welds, and other mechanical fasteners. Seals and bonds in one step. 4.. |
|||
Tensile Strength, Ultimate | 3.79 MPa | 550 psi | |
Dow Corning HS II BASE & 10:1, COLORED CATALYST High strength silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items and better suited for thin section cure. HS II Base with HS II 10:1 Colored C.. |
|||
Tensile Strength, Ultimate | 3.79 MPa | 550 psi | |
Dow Corning HS II BASE & SPRAYABLE COLORED CATALYST High strength silicone mold making rubber, suited for the reproduction of robotic skins, tooling and immovable objects due to its thixotropic characteristics. HS II Base with HS Sprayable Catalyst C.. |
|||
Tensile Strength, Ultimate | 3.79 MPa | 550 psi | |
Dow Corning SILASTIC® HV 1666/65 GRAY SILICONE RUBBER 65 Durometer, gray, peroxide cure, high voltage grade Silicone Rubber Compound for manufacturing High Voltage insulators weather shed insulators or surge arrestors. Superior wet electrical propertie.. |
|||
Tensile Strength, Ultimate | 3.79 MPa | 550 psi | |
Dow Corning SILASTIC® L RTV SILICONE RUBBER BASE & CURING AGENT Low durometer silicone mold making rubber recommended for use with rigid polyurethanes and can be used with polyesters and epoxies.Information provided by Dow Corning |
|||
Tensile Strength, Ultimate | 3.79 MPa | 550 psi | |
Loctite® Nuva-Sil® 5084 Sealant Silicon Light Cure Adhesives and Gasketing and Wire TackersLoctite® innovative gasketing products offer precise, reliable sealing of electronic enclosures, protecting them from environmental hazard.. |