Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 300 MPa @Temperature 700 °C |
43500 psi @Temperature 1290 °F |
EN min. |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Ultimate | 300 MPa @Temperature 600 °C |
43500 psi @Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4878 High Temperature Austenitic Stainless Steel Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For .. |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | |
Pacific Sintered Materials FN-252-S Iron Nickel Soft Magnetic Powdered Metal Very low coercive force and high permeability. Excellent for shielding and switching applications.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | |
PSM Industries Pacific Sintered Metals Iron Nickel FN-252-S Powdered Metal Very low coercive force and high permeability. Excellent for shielding and switching applications.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 300 - 500 MPa | 43500 - 72500 psi | |
MMCC Al/Al2O3 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | 300 - 500 MPa | 43500 - 72500 psi | |
MMCC Al/Al2O3 Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | 300 - 450 MPa | 43500 - 65300 psi | |
MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | 300 - 500 MPa | 43500 - 72500 psi | |
MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | 300 - 500 MPa | 43500 - 72500 psi | |
MMCC Cu/B4C Particulate Copper Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | >= 300 MPa | >= 43500 psi | |
H.C. Starck MoCu 80/20 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
Tensile Strength, Ultimate | 300 - 450 MPa | 43500 - 65300 psi | |
MMCC Al/SiC Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | Longitudinal |
Special Metals Electroformed Nickel, 13 Micron (0.5 mil) Foil, Electroformed and Annealed Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | |
Sapco 99.9% Aluminum Oxide Information provided by Sapco. |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | |
Wieland 1601 Wilaform Gold Soft yellow gold alloy, ideally for the production of strongly deformed parts in decoration manufacturing and for metal coinage.Applications: casting, chains, coin/shape, laminar decoration, pipes, .. |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | |
Wieland 1703 Wilaform Gold Yield alloy particularly suitable for coin and medal production.Applications: casting, chains, coin/shape, laminar decoration, tubingDental |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | |
Wieland 3012 Wilaform Silver A balance of manufacturing and performance characteristics makes this the preferential silver alloy in the decoration manufacturing industry. The alloy unites good ductility properties with the nec.. |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | ASTM D638 |
Hexcel® HexMC™ C / 2000 / R1 Composite SMC High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications.. |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | |
China Tungsten STG90-30 PM Structural Parts Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | .0275 - .035 inches sheet thickness; ASTM A 370 |
AK Steel ASTM A 424 Type 1, UNIVIT® DS Enameling Carbon Steel UNVIT is a specialty enameling steel developed for applications where direct-on cover coat enameling is employed. This product is free of porcelain enamel fishscale regardless of the enameling syst.. |
|||
Tensile Strength, Ultimate | >= 300 MPa | >= 43500 psi | |
Aleris Alustar Aluminum Alloy, MIG-welded At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d.. |
|||
Tensile Strength, Ultimate | 300 MPa | 43500 psi | |
Ametek Ultra 316L P/M Stainless Steel, Sintered from 6.49 g/cc Green Density Ametek's patented Ultra Stainless Steels™ are produced by alloying the conventional austenitic compositions with a small amount of a copper-nickel-tin alloy. This results in a marked improvement i.. |
|||
Tensile Strength, Ultimate | 300 - 400 MPa | 43500 - 58000 psi | |
ArcelorMittal 13 High formability steel for drawing, Hot rolled Available in the following: uncoated (DD13) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au.. |
|||
Tensile Strength, Ultimate | 300 - 360 MPa | 43500 - 52200 psi | |
ArcelorMittal 180 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC180B), electroglavanized (HC180B+ZE) and Extragal®/Galvannealed (HC180BD+Z)Description: The composition and processing of these steels are designed to promot.. |
|||
Tensile Strength, Ultimate | >= 300 MPa | >= 43500 psi | |
AK Steel Cold Rolled Carbon Steel, Bake Hardenable (BH 180), SAE J2340 Type 180 B Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 300 MPa @Temperature 600 °C |
43500 psi @Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 4948 High Temperature Austenitic Stainless Steel Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for.. |
|||
Tensile Strength, Ultimate | 300 MPa @Temperature 870 °C |
43500 psi @Temperature 1600 °F |
|
Haynes Hastelloy® alloy 625 12.7 mm plate weldments Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |