Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 290 MPa | 42000 psi | Typical |
PSM Industries PolyAlloys MIM-2200 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 290 MPa | 42000 psi | |
PSM Industries PolyAlloys MIM-2200 Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 289.6 MPa | 42000 psi | |
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%.. |
|||
Tensile Strength, Ultimate | 290 MPa | 42000 psi | |
MTI ThermoStran® PA66-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 290 MPa | 42000 psi | |
MTI ThermoStran® PPA-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 290 MPa | 42000 psi | Transverse |
Special Metals Electroformed Nickel, 13 Micron (0.5 mil) Foil, Electroformed and Annealed Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 290 - 359 MPa | 42000 - 52000 psi | |
Eagle Brass 210 Gilding Metal, 1/2 Hard CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Ultimate | 290 MPa | 42000 psi | |
Ametek P316L P/M Stainless Steel, Sintered from 6.25 g/cc Green Density P316L offers a very high degree of corrosion protection for a standard P/M stainless steel grade. It provides excellent strength at extremely high temperatures. Key materials benefits of P316L inclu.. |