Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | 2 in/min.; ASTM D638 |
Ineos H20A-00 Polypropylene Homopolymer A controlled rheology polypropylene homopolymer produced by Ineos utilizing unique catalyst technology. It is designed for injection molding applications requiring a moderate level of antistatic ag.. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | |
Kraton® D1102 + PP blend (25/75) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ASTM D638 |
KKPC Kuhmo HI 425 General Purpose HIPS Key features: High-impact General Use. Common Uses: Office appliances, home appliances, various kitchenware, general merchandise, toys, leisure goods, etc.HIPS is a functional resin made by copolym.. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ASTM D638 |
KKPC Kuhmo HI 425TVL High Flow/High Heat Resistant HIPS Key features: Super high-fluidity. Common Uses: TV cover (Fine TV), Drawers.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-.. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ASTM D638 |
American Polymers API 550 HF Polystyrene API 550 HF is a high impact grade of polystyrene. It is characterized by good impact and processability. API 550 HF offers good retention of mechanical properties in applications with long flow le.. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ASTM D638 |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ASTM Data |
Dow Retain® PS-4378 Polystyrene Data provided by Dow Chemical. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ASTM D638 |
Colorite Polymers 1194B General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | Bond strength to glass |
Dymax Light Weld® 401 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ASTM D638 |
Adell EZ-16 Homopolymer Polypropylene, 30% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | 0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638 |
Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion ap.. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ACMA Test #4 |
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2) Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America. |
|||
Tensile Strength, Ultimate | 25.5 MPa | 3700 psi | ASTM D638 |
Adell RA-18 Copolymer Polypropylene, 40% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 25.5 - 65.5 MPa | 3700 - 9500 psi | Average value: 43.7 MPa Grade Count:9 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |