Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.7 MPa
2710 psi
Freudenberg Simrit Simriz® 487 High Temperature FFKT Perfluoroelastomer Compound
Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of ..
Tensile Strength, Ultimate 18.7 MPa
2710 psi
Original Properties; ASTM D412 Die C
Freudenberg Simrit N475 Nitrile Elastomer (NBR)
General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings
Tensile Strength, Ultimate 18.7 MPa
2710 psi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8605 (GF-S), VTR 8600 (GF-S) 8605/VTR 8600 Blend  (discontinued **)
FormulationVTR 8605