Polymer Property : Tensile Strength, Ultimate = 2480 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.1 MPa
2480 psi
Freudenberg Simrit Simriz® 481 Low Temperature FFKT Perfluoroelastomer Compound
Perfluoro elastomers – or FFKM for short – have an ideal combination of characteristics, with their excellent chemical resistance, high level of temperature resistance, and high levels of ..