Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | |
Sylvin Technologies 8940-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | |
Sylvin Technologies 8960-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | |
Sylvin Technologies 916V0 Black PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | |
Sylvin Technologies 9600-85 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | |
Sylvin Technologies 9940-80 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | |
Sylvin Technologies 9960-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | ASTM-D1457 |
CoorsTek PolyGlyde™ 3000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | ASTM D412 |
Colorite Polymers CS7541GP Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | ASTM D412 |
Colorite Polymers CS8039UL Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | ASTM D638 |
Colorite Polymers MULTICHEM™ 8514 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | ASTM D638 |
Colorite Polymers 7000-UV General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | ASTM D412 |
Colorite Polymers CS1542OR Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | ASTM D638 |
Colorite Polymers 7000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Tensile Strength, Ultimate | 15.5 MPa | 2250 psi | |
Sylvin Technologies 6149-80 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |