Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1517 - 1689 MPa | 220000 - 245000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH8, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Ultimate | 1520 MPa | 220000 psi | 50% Cold Rolled |
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
Tensile Strength, Ultimate | 1520 MPa | 220000 psi | 700°F Temper Temperature |
Latrobe Lescalloy® 4335+V VAC-ARC High Strength Alloy Steel 4335+V VAC-ARC is a low alloy steel with good strength and high hardenability. In addition, uniform properties are obtained in large sections. The alloy can be heat treated to strength values with.. |
|||
Tensile Strength, Ultimate | 1520 MPa | 220000 psi | 24°C Test Temp |
Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe.. |
|||
Tensile Strength, Ultimate | >= 1520 MPa | >= 220000 psi | H950 Condition - 500°C |
Latrobe Lescalloy® 13-8 Mo VIM-VAR Precipitation Hardening Stainless Steel Lescalloy 13-8 Mo VIM-VAR is a precipitation hardening martensitic stainless steel offering excellent fracture toughness and transverse mechanical properties coupled with the resistance to stress-co.. |
|||
Tensile Strength, Ultimate | 1517 MPa | 220000 psi | |
HP Alloys Alloy 718, 15% Cold Worked, Aged 15% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Tensile Strength, Ultimate | 1520 MPa | 220000 psi | |
Specialty Materials 5521 Boron Epoxy Prepreg Tape Specialty Materials' 5521 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Performing at temperatures up to 350°F,.. |
|||
Tensile Strength, Ultimate | 1520 MPa | 220000 psi | Aged to ~ 46 HRC |
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli.. |
|||
Tensile Strength, Ultimate | 1517 MPa | 220000 psi | |
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition C AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
Tensile Strength, Ultimate | 1517 MPa | 220000 psi | |
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition C AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
Tensile Strength, Ultimate | 1517 MPa | 220000 psi | |
ATI Allegheny Ludlum AL 13-8™ H 950 Precipitation Hardening Alloy Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Tensile Strength, Ultimate | 1517 MPa | 220000 psi | |
ATI Allvac® 720 Nickel Superalloy, Heat Treatment: 1093°C (2000°F) + Age Data provided by Allvac.Applications: Wheels, jet engine turbine discs and blades. |
|||
Tensile Strength, Ultimate | 1517 MPa | 220000 psi | |
ATI Allvac® Vasco® 455 Specialty Steel, Heat Treatment: 829°C (1525°F) + Age Data provided by Allvac.Applications: High-strength aircraft components including fasteners, bolts, pins, pressure vessels, gears, shafts. |
|||
Tensile Strength, Ultimate | 1517 MPa | 220000 psi | |
ATI Allvac® Vasco® 9-4-30 Specialty Steel, Heat Treatment: 899°C (1650°F) + Age Data provided by Allvac.Applications: Aircraft structural components, rocket motor cases, pressure vessels, armor applications. |
|||
Tensile Strength, Ultimate | 1517 MPa @Temperature -73.0 °C |
220000 psi @Temperature -99.4 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Tensile Strength, Ultimate | 1520 MPa | 220000 psi | |
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel LESCALLOY HY-TUF VAC-ARC steel is a high strength low alloy steel. It is typically used in the 220/240 ksi (1517/1655 MPa) tensile strength range. At this strength level, the alloy has good ductilit.. |
|||
Tensile Strength, Ultimate | 1520 MPa | 220000 psi | Oil Quenched from 871°C; 538°C Temper Temperature |
Latrobe Staminal™ Shock Resisting Die Steel Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, .. |