Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1390 MPa | 202000 psi | |
Haynes 230® alloy, 40% cold reduction Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic.. |
|||
Tensile Strength, Ultimate | 1390 MPa @Temperature 595 °C |
202000 psi @Temperature 1100 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Ultimate | 1390 - 1400 MPa | 202000 - 203000 psi | |