Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1280 MPa | 185000 psi | |
FloMet 17-4PH Stainless Steel, Heat Treated (H-900) FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Ultimate | 1280 MPa | 185000 psi | |
Materion moldMAX® HH High Hardness Beryllium Copper Alloy Description: moldMAX® and PROtherm® are Brush Wellman's copper beryllium alloys specifically designed for the plastic processing industry. These alloys provide a combination of thermal con.. |
|||
Tensile Strength, Ultimate | 1280 MPa | 185000 psi | hardened to 40 HRC |
Bohler-Uddeholm BeCu Alloy 172 Mold Material Beryllium copper alloyA high strength beryllium copper mold alloy with high thermal conductivity.BeCu Alloy 172 is characterized by: High thermal conductivity Good corrosion resistance Good polisha.. |
|||
Tensile Strength, Ultimate | 1280 MPa | 185000 psi | |
AIM 88Au/12Ge Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |