Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 91.0 MPa | 13200 psi | ASTM D638 |
Toyobo T-423 Nylon, Mineral-Reinforced Key Feature: High heat distortion and good toughness, good surfaceInformation provided by Toyobo Co., Ltd |
|||
Tensile Strength, Ultimate | 91.0 MPa | 13200 psi | ISO 527-1, 2 |
Polyplastics Duranex® 3116 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 7.5% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 91.0 MPa | 13200 psi | ASTM D638 |
Toyobo T-422T Nylon, Mineral-Reinforced Key Feature: High heat distortion and good toughnessInformation provided by Toyobo Co., Ltd |
|||
Tensile Strength, Ultimate | 91.0 MPa | 13200 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 273 Polystyrene Alloy, Glass Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 91.0 MPa @Temperature 60.0 °C |
13200 psi @Temperature 140 °F |
ISO 527 |
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Tensile Strength, Ultimate | 91.0 MPa @Temperature 1149 °C |
13200 psi @Temperature 2100 °F |
|
Haynes 230® alloy, hot rolled and 1232°C solution annealed plate Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat.. |
|||
Tensile Strength, Ultimate | 91.0 MPa | 13200 psi | ISO 527-1, 2 |
Polyplastics Duracon® KT-20 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Wear resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |