Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.96 MPa
1300 psi
as molded
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.96 MPa
1300 psi
TM R050-36
Resinlab® EP1225 Black Unfilled Epoxy Adhesive
Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
post cured- 4 hours at 177°C; ASTM D412
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.96 MPa
1300 psi
post cured- 8 hours at 177°C; ASTM D412
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.96 MPa
1300 psi
post cured- 2 hours at 177°C; ASTM D412
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.96 MPa
1300 psi
post cured- 8 hours at 177°C; ASTM D412
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.96 MPa
1300 psi
post cured- 2 hours at 177°C; ASTM D412
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.96 MPa
1300 psi
post cured- 4 hours at 177°C; ASTM D412
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.96 MPa
1300 psi
post cured- 8 hours at 177°C; ASTM D412
Multibase C6-250 VAROX DBPH Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Sylvin Technologies 8940-60 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Sylvin Technologies 9077-65 Natural PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Sylvin Technologies 9940-60 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Sylvin Technologies 5100 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 8.96 MPa
1300 psi
ASTM D638
Westlake EC476AA Low Density Polyethylene
WESTLAKE polyethylene EC476 is a low-density resin designed for applications where high coating speeds and good drawdown are required. This material demonstrates good adhesion to paper, provides a g..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
ASTM D638
Westlake EC477AA Low Density Polyethylene
WESTLAKE polyethylene EC477 is a low-density resin designed for applications where high coating speeds and good drawdown are required. This material demonstrates good adhesion to paper, provides a g..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation
Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Dow Corning SILASTIC® LS 4-9038 FLUOROSILICONE RUBBER
50 Durometer, off-white, uncatalysed, high temperature grade fluorosilicone base.Information provided by Dow Corning
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Dow Corning SILASTIC® Q7-4720 BIOMEDICAL GRADE ETR ELASTOMER, KIT
Two-part, platinum-catalyzed (1:1 by weight), enhanced tear-resistant silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices.I..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
ASTM D638
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer
AFFINITY™ EG 8150G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene alpha-olefin copolymer exhibiting high flexibility and elasticity. It can be ut..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
ASTM D-638
CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products
CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume prod..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
ASTM D638
Colorite Polymers Elastichem 4011TX-02 Vinyl Compound
Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Colorite Polymers 5012 Clear Injection Molding Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Bond strength to metal
Dymax Light Weld® 402 High Clarity Glass Bonding Adhesive
Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
ASTM D412; ISO 37
Advanced Polymer Alloys Alcryn® 3065 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 3065 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
Colorite Polymers 5011 Clear Extrusion Vinyl Compound
Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre..
Tensile Strength, Ultimate 8.96 MPa
1300 psi
TM R050-36
Resinlab® EP1026R Rubber Modified Epoxy Adhesive
Resinlab™ EP1026R is a two part unfilled rubber modified epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free ..