Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.80 MPa | 1280 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 7301 BLK The data is the actual data obtained from the above sample. This material is based on Shell's Kraton G technology. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 8.83 MPa | 1280 psi | no post cure, press cured for 5 minutes; ASTM D412 |
Multibase SILASTIC® 7-4860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Ultimate | 8.83 MPa | 1280 psi | no post cure, press cured for 5 minutes; ASTM D412 |
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tensile Strength, Ultimate | 8.83 MPa | 1280 psi | no post cure; ASTM D412 |
Multibase C6-560 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 8.83 MPa | 1280 psi | ASTM D412 |
Stellarchem SV-B75E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Tensile Strength, Ultimate | 8.83 MPa | 1280 psi | |
Dow Corning C6-560 LIQUID SILICONE RUBBER KIT Dow Corning® Class VI Elastomers are heat cured elastomer raw materials for use by customers fabricating medical devices and parts.Information provided by Dow Corning |
|||
Tensile Strength, Ultimate | 8.83 MPa | 1280 psi | |
Dow Corning SILASTIC® 7-4860 BIOMEDICAL GRADE LSR, KIT Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning |
|||
Tensile Strength, Ultimate | 8.83 MPa | 1280 psi | |
Dow Corning SILASTIC® 7-6830 BIOMEDICAL GRADE LSR, KIT Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning |
|||
Tensile Strength, Ultimate | 8.80 MPa | 1280 psi | ISO 527-1/-2 |
DSM Arnitel® XG5858 TPC-ET Injection Molding |
|||
Tensile Strength, Ultimate | 8.80 MPa | 1280 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8180 Polyolefin Elastomer Description: Engage® 8180 polyolefin elastomer is a lower density, high performance ethylene-octene copolymer that has excellent flow characteristics and provides good impact properties in blends w.. |
|||
Tensile Strength, Ultimate | 8.80 MPa | 1280 psi | |
Dow LDPE 955I Low Density Polyethylene DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid.. |
|||
Tensile Strength, Ultimate | 8.83 MPa | 1280 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |