Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | TM R050-36 |
Resinlab® EP1121-4 Adhesive / Casting Resin Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives .. |
|||
Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | |
Dow Corning SILASTIC® Q7-4565 BIOMEDICAL GRADE ETR ELASTOMER One-part, enhanced tear-resistant silicone elastomers; uncatalyzed (customer selects peroxide catalyst) elastomer materials designed for compounding into elastomer for part fabrication and medical d.. |
|||
Tensile Strength, Ultimate | >= 7.90 MPa | >= 1150 psi | |
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51946C015) Cured silicone rubber with a minimum thickness of 0.002 in. (0.05 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.005 in. (0.1 mm); 0.003 i.. |
|||
Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | silicone property; ASTM D412 |
Arlon 55946C028 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The foll.. |
|||
Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | cured 30 days @ 25°C |
Abatron AboCast 8110-2/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | silicone property; ASTM D412 |
Arlon 56946C026 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Tensile Strength, Ultimate | 7.93 MPa | 1150 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 7.93 - 45.5 MPa | 1150 - 6600 psi | Average value: 12.6 MPa Grade Count:38 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |