Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.40 MPa | 1070 psi | |
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound
& Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. .. |
|||
Tensile Strength, Ultimate | 7.36 - 191.87 MPa @Temperature -40.0 - 150 °C |
1070 - 27828 psi @Temperature -40.0 - 302 °F |
Average value: 61.4 MPa Grade Count:2 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Tensile Strength, Ultimate | 7.36 - 191.87 MPa @Strain 0.180 - 160 % |
1070 - 27828 psi @Strain 0.180 - 160 % |
Average value: 61.4 MPa Grade Count:2 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Tensile Strength, Ultimate | 7.40 MPa | 1070 psi | |
Kuraray SEPTON® S45 Soft Compound Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre.. |
|||
Tensile Strength, Ultimate | 7.35 MPa | 1070 psi | ASTM D412 |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Tensile Strength, Ultimate | 7.40 - 31.8 MPa | 1070 - 4610 psi | Average value: 19.3 MPa Grade Count:42 |
Overview of materials for Chlorosulfonated Polyethylene Rubber This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val.. |