Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 69.57 MPa | 10090 psi | Type 1 - Rigids, 0.2 in/min, 50% in/in; ASTM D638 |
PolyOne Therma-Tech™ NJC-5000 TC NATURAL Nylon 12
(discontinued **) Information provided by PolyOne Corporation. |