Polymer Property : Tensile Strength, Ultimate = 97.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 83.0 - 97.0 MPa
12000 - 14100 psi
Average value: 90.0 MPa Grade Count:7
Overview of materials for Epoxy, Molded, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Ultimate 5.17 - 97.0 MPa
750 - 14100 psi
Average value: 33.7 MPa Grade Count:31
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 75.0 - 97.0 MPa
10900 - 14100 psi
ASTM D638
Zeus PEEK Tubing
PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used..