Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 580 - 830 MPa | 84100 - 120000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 25 to 51 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 580 - 830 MPa | 84100 - 120000 psi | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 580 - 830 MPa | 84100 - 120000 psi | |
Materion Beryllium Copper Alloy 165 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 750 - 830 MPa | 109000 - 120000 psi | |
Materion Beryllium Copper Alloy 190 Strip; 1/4HM (TM01) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Ultimate | 580 - 830 MPa | 84100 - 120000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 580 - 830 MPa | 84100 - 120000 psi | |
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 680 - 830 MPa | 98600 - 120000 psi | |
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl.. |
|||
Tensile Strength, Ultimate | 580 - 830 MPa | 84100 - 120000 psi | |
Materion Beryllium Copper Alloy 25 Tube; H (TD04) Temper; 0ver 25.4 to 76 mm o.d. (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 680 - 830 MPa | 98600 - 120000 psi | |
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; AT (TF00) Temper (UNS C17510) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Ultimate | 580 - 830 MPa | 84100 - 120000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 580 - 830 MPa | 84100 - 120000 psi | |
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 680 - 830 MPa | 98600 - 120000 psi | |
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; AT (TF00) Temper (UNS C17500) Treatment required for max strength: 3 hrs @ 480°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc... |