Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 770 - 780 MPa | 112000 - 113000 psi | |
Kennametal Stellite Denertia™ C14 Cobalt Chromium Dental Alloy Denertia™ C14 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework. It conforms to the following International Standards: EN 1641 §.. |
|||
Tensile Strength, Ultimate | 580 - 780 MPa | 84100 - 113000 psi | Minimum Guaranteed |
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Tensile Strength, Ultimate | 770 - 780 MPa | 112000 - 113000 psi | |
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy Denertia™ C4 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.It conforms to the following International Standards: EN 1641 §4... |
|||
Tensile Strength, Ultimate | 570 - 780 MPa | 82700 - 113000 psi | |
CLAL-MSX NICLAL 1300 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX |