Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 10 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 10 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Forgings & Extrusions; A (TB00) Temper (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Wire; A (TB00) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; A (TB00) Temper (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17500)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 270 - 380 MPa
39200 - 55100 psi
ArcelorMittal 53+AS Aluminized steel
Use: Difficult drawingInformation provided by ArcelorMittal
Tensile Strength, Ultimate 240 - 380 MPa
34800 - 55100 psi
Materion Beryllium Copper Alloy 3 Tube; A (TB00) Temper; All Sizes (UNS C17510)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..