Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 50.0 - 228 MPa | 7250 - 33000 psi | Average value: 68.5 MPa Grade Count:33 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 45.0 - 228 MPa | 6530 - 33000 psi | Average value: 65.6 MPa Grade Count:156 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 62.1 - 228 MPa | 9000 - 33000 psi | Average value: 161 MPa Grade Count:37 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |