Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1310 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1170 - 1310 MPa
170000 - 190000 psi
Solution Annealed & Aged
Materion Beryllium Nickel M220C
Information supplied by Brush Wellman Engineered Materials.Brush M220C is characterized by high levels of strength, hardness, and thermal conductivity combined with excellent resistance to wear, cor..
Tensile Strength, Ultimate 1070 - 1310 MPa
155000 - 190000 psi
Materion Beryllium Nickel Strip - Alloy 360 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way)..
Tensile Strength, Ultimate 1030 - 1310 MPa
150000 - 190000 psi
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar
Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic..
Tensile Strength, Ultimate 1100 - 1310 MPa
160000 - 190000 psi
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or..
Tensile Strength, Ultimate 1100 - 1310 MPa
160000 - 190000 psi
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire
Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i..
Tensile Strength, Ultimate 1070 - 1310 MPa
155000 - 190000 psi
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al..
Copyright © lookpolymers.com All Rights Reserved