Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 28.0 - 116 MPa @Temperature -40.0 - 80.0 °C |
4060 - 16800 psi @Temperature -40.0 - 176 °F |
Average value: 73.0 MPa Grade Count:2 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 24.0 - 116 MPa @Temperature -40.0 - 80.0 °C |
3480 - 16800 psi @Temperature -40.0 - 176 °F |
Average value: 49.1 MPa Grade Count:6 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |