Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 9.28 - 138 MPa @Temperature -20.0 - 200 °C |
1350 - 20000 psi @Temperature -4.00 - 392 °F |
Average value: 49.7 MPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Tensile Strength, Ultimate | 9.28 - 138 MPa @Strain 0.230 - 4.21 % |
1350 - 20000 psi @Strain 0.230 - 4.21 % |
Average value: 49.7 MPa Grade Count:1 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |