Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 882.6 MPa | >= 128000 psi | |
Crucible Steel 21-2N Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | >= 882.6 MPa | >= 128000 psi | |
Crucible Steel 21-4N (JIS SUH35) Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | >= 882.6 MPa | >= 128000 psi | |
Crucible Steel 21-4NNb Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | >= 882.6 MPa | >= 128000 psi | |
Crucible Steel 23-8N Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | >= 882.6 MPa | >= 128000 psi | |
Crucible Steel 422 (JIS SUH616) Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | >= 882.6 MPa | >= 128000 psi | |
Crucible Steel SUE52 Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | >= 882.6 MPa | >= 128000 psi | |
Crucible Steel 214NS (JIS SUH36) Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | >= 882.6 MPa | >= 128000 psi | |
Crucible Steel SIL 10N Martensitic Steel Information provided by Crucible Specialty Metals. |