Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.80 MPa | 1280 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 7301 BLK The data is the actual data obtained from the above sample. This material is based on Shell's Kraton G technology. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 8.80 MPa | 1280 psi | ISO 527-1/-2 |
DSM Arnitel® XG5858 TPC-ET Injection Molding |
|||
Tensile Strength, Ultimate | 8.80 MPa | 1280 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8180 Polyolefin Elastomer Description: Engage® 8180 polyolefin elastomer is a lower density, high performance ethylene-octene copolymer that has excellent flow characteristics and provides good impact properties in blends w.. |
|||
Tensile Strength, Ultimate | 8.80 MPa | 1280 psi | |
Dow LDPE 955I Low Density Polyethylene DOW LDPE 955I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility, and good toughness, with low warpage. Typical applications include lid.. |