Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.48 MPa | 1230 psi | post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 8.48 MPa | 1230 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 283-40MED Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tensile Strength, Ultimate | 8.48 - 80.0 MPa | 1230 - 11600 psi | Average value: 16.6 MPa Grade Count:51 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Ultimate | 8.48 MPa | 1230 psi | post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-515 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 8.48 MPa | 1230 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 8.48 MPa | 1230 psi | |
Dow Corning SILASTIC® LS 5-8720 FLUOROSILICONE RUBBER 20 Durometer, off-white, Fluorosilicone Base.Information provided by Dow Corning |