Polymer Property : Tensile Strength, Ultimate = 7.963 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.963 MPa
1155 psi
post cured- 4 hours at 204°C
Multibase SILASTIC® C7-4565 TBPB Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 7.963 MPa
1155 psi
post cured- 2 hours at 177°C; ASTM D412
Multibase C6-350 LH Parts A and B Dow-Corning Class VI Elastomer
Information provided by Multibase