Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.274 MPa
1055 psi
post cured- 4 hours at 177°C; ASTM D412
Multibase C6-165 Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Ultimate 7.274 MPa
1055 psi
Dow Corning SILASTIC® LC-30-2004 PART A&B KIT
30 Durometer, 2 parts, 1 to 1 mix, translucent, FDA 21 CFR 177.2600 and BfR, XV, molding and injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning