Polymer Property : Tensile Strength, Ultimate = 669 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 669 - 772 MPa
97000 - 112000 psi
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Ultimate 669 MPa
97000 psi
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Tensile Strength, Ultimate 669 MPa

@Temperature 70.0 °C
97000 psi

@Temperature 158 °F
transverse
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-8 (UNS S20153)
AL 201LN™ is a special composition of Type 201 specifically for sub-zero temperature service as welded tanks and vessels. This alloy has replaced the familiar 300 series stainless such as type 301..