Polymer Property : Tensile Strength, Ultimate = 634 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 634 MPa

@Temperature 316 °C
92000 psi

@Temperature 601 °F
Haynes HR-160® alloy, hot rolled and solution annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Tensile Strength, Ultimate 634 MPa

@Temperature 316 °C
92000 psi

@Temperature 601 °F
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Ultimate >= 634 MPa
>= 92000 psi
Eagle Brass 425 Tin Brass 2%, Extra Spring
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Ultimate 634 - 738 MPa
92000 - 107000 psi
Eagle Brass 64725 MAX251C, Extra Hard
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In..
Tensile Strength, Ultimate 634 - 738 MPa
92000 - 107000 psi
Eagle Brass 770 Nickel Silver 18%, Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Tensile Strength, Ultimate 634 MPa

@Temperature 427 °C
92000 psi

@Temperature 801 °F
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..