Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 427 MPa | 62000 psi | |
Kinetics MIM F15 (Kovarâ„¢) Low CTE Alloy High nickel, high cobalt iron alloy. A traditional metal-to- glass sealing alloy that offers a low coefficient of thermal expansion (CTE) similar to glass. Provides the hermeticity required for firm.. |
|||
Tensile Strength, Ultimate | 427 MPa @Diameter 12.7 mm |
61900 psi @Diameter 0.500 in |
|
Kaiser 4026 T651 Rod & Bar This alloy is used when high strength with wear and/or galling resistance is required. It can eliminate hard-coat anodizing in some applications. Typical applications include air compressor pistons .. |
|||
Tensile Strength, Ultimate | 427 - 510 MPa | 62000 - 74000 psi | |
Eagle Brass 425 Tin Brass 2%, 3/4 Hard Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector.. |
|||
Tensile Strength, Ultimate | 427 MPa | 62000 psi | Fully Processed |
AK Steel DI-MAX® M-47 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Tensile Strength, Ultimate | 427 MPa | 62000 psi | ASTM D638 |
Applied Composites 8068 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Structural Grade Chopped and Unidirectional Fibers, High Stiffness, High Fiber LoadingsInformation provided by Appl.. |