Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 414 MPa | 60000 psi | Typical |
PSM Industries PolyAlloys MIM-2700 sintered Low Alloy Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | Typical |
PSM Industries PolyAlloys MIM-430L sintered Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | |
Kennametal Stellite Delcrome® 93 Information provided by Deloro Stellite, Inc. Typical data, not guaranteed as a maximum or minimum. Highly alloyed white cast iron, abrasion resistant. Carbides in a martensitic matrix offer high.. |
|||
Tensile Strength, Ultimate | 414 MPa @Temperature 760 °C |
60000 psi @Temperature 1400 °F |
|
Kennametal Stellite Stellite® 31 PM with P/M Processing; heat treated at 93°C (200°F) and water quenched Typical applications include, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | |
FloMet Fe-50% Ni Soft Magnetic Alloy FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume.. |
|||
Tensile Strength, Ultimate | 414 - 517 MPa | 60000 - 75000 psi | |
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 414 - 552 MPa | 60000 - 80000 psi | |
Meehanite Almanite® WS Wear and Abrasion Resisting Cast Iron Type WS is a hard wearing martensitic iron with exceptional impact strength...not readily machinable...work hardens in service to high hardness values. Type WS is recommended for crusher jaws, impa.. |
|||
Tensile Strength, Ultimate | 414 - 689 MPa | 60000 - 100000 psi | |
Meehanite CHS Corrosion Resisting Cast Iron Type CHS is a higher strength material with good shock resistance. Compositional adjustments are made to suit exact service requirements. Recommended for use for components subjected to concentrat.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | |
Meehanite GM-60 Flake Graphite Cast Iron Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a.. |
|||
Tensile Strength, Ultimate | 414 - 689 MPa | 60000 - 100000 psi | |
Meehanite HS Heat Resisting Cast Iron Type HS compares very favorably from a strength standpoint with any heat resisting metal. Compositional adjustments are made to suit the exact service conditions. It machines easily and provides m.. |
|||
Tensile Strength, Ultimate | 414 MPa @Diameter 12.7 mm |
60000 psi @Diameter 0.500 in |
|
Kaiser 6033 T6, T651 Rod & Bar Alloy 6033 is a higher strength version of alloy 6061, approaching properties typically obtainable with 2000 series alloys. The alloy was developed to also offer improved machinability over 6061. Th.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | Stainless Steel (18-8) Annealed butt joint |
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin.. |
|||
Tensile Strength, Ultimate | 414 - 552 MPa | 60000 - 80000 psi | |
Meehanite Almanite® W4 Wear and Abrasion Resisting Cast Iron Type W4 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W4 is highly alloyed to provide an austenitic matrix in the as-cast conditio.. |
|||
Tensile Strength, Ultimate | 414 MPa @Diameter 12.7 mm |
60000 psi @Diameter 0.500 in |
|
Kaiser 4026 T8 Rod & Bar This alloy is used when high strength with wear and/or galling resistance is required. It can eliminate hard-coat anodizing in some applications. Typical applications include air compressor pistons .. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | |
Universal Wire Works 505 E8018-B8 Stainless Steel Electrode Universal 505 electrodes deposit 9% chromium 1% molybdenum deposits in applications that are primarily pipe, tube and castings. Type 505 is an air hardening alloy and as such requires both a preheat.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | |
Universal Wire Works 61 Nickel Alloy Welding Wire Alloy 61 is used for TIG, MIG, and submerged-arc welding of Nickel 200 and 201, and for overlaying on steel. There is a reaction of carbon with titanium during the welding process so there is a low .. |
|||
Tensile Strength, Ultimate | 414 - 483 MPa | 60000 - 70000 psi | |
Eagle Brass 19210 XP-10 Copper Iron, Extra Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Ultimate | 414 - 483 MPa | 60000 - 70000 psi | |
Eagle Brass 194 HSM® Copper, Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Ultimate | 414 - 469 MPa | 60000 - 68000 psi | |
Eagle Brass 210 Gilding Metal, Spring CDA 210 is known for its resistance to corrosion. The alloy also lends itself to deep drawing such as bullet jackets and electrical applications where formability and conductivity are required. Typi.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | Forging (Hot Forged and Heat Treated) |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Tensile Strength, Ultimate | >= 414 MPa | >= 60000 psi | Mid-radius |
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | annealed |
CMW® ELKONIUM 305 platinum based alloy Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | cold worked |
CMW® ELKONIUM 72 gold based alloy Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to .. |
|||
Tensile Strength, Ultimate | >= 414 MPa | >= 60000 psi | Specification |
AK Steel 18 Cr-Cb™ Ferritic Stainless steel AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili.. |
|||
Tensile Strength, Ultimate | 414 - 552 MPa | 60000 - 80100 psi | |
Ametek High Purity Nickel Strip 899A 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 414 - 552 MPa | 60000 - 80100 psi | |
Ametek High Purity Nickel Strip 899L 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 414 - 552 MPa | 60000 - 80100 psi | |
Ametek High Purity Nickel Strip 899M 1/2 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | >= 414 MPa | >= 60000 psi | |
AK Steel 444 Ferritic Stainless steel AK Steel 444 is a low-carbon, low nitrogen, ferritic stainless steel that provides pitting and crevice corrosion resistance superior to most ferritic stainless steels. Applications requiring superi.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-S Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-35Information Provided by Pacific Sintered Metals, a division.. |
|||
Tensile Strength, Ultimate | 414 MPa | 60000 psi | |
PSM Industries PolyAlloys MIM-430L sintered Soft Magnetic Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |