Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 4137 MPa | 600000 psi | |
Zoltek Panex 35® 50k Continuous Tow Commercial Carbon Fiber for Industrial Applications Commercial Carbon Fiber for Industrial Applications |
|||
Tensile Strength, Ultimate | 4137 MPa | 600000 psi | |
Zoltek Panex 35® Tow Weave Carbon Fiber Fabrics Tow Weave Carbon Fiber Fabrics |