Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 372 MPa
54000 psi
Kinetics MIM 12 Chrome
Stainless Steel for soft magnetic applications. Information provided by Kinetics, Inc.
Tensile Strength, Ultimate 372 MPa

@Temperature 760 °C
54000 psi

@Temperature 1400 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Ultimate >= 372 MPa
>= 54000 psi
Alcoa Toolrite 2011®-T8 Aluminum
Weldability = D; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting ..
Tensile Strength, Ultimate 372 MPa
54000 psi
CMW® DSC Copper with Dispersed Aluminum Oxide
CMW® DSC material is an extruded and cold worked powder metallurgy material consisting of copper and dispersed aluminum oxide. It has exceptional high temperature strength for its electrical conduc..
Tensile Strength, Ultimate 372 MPa
54000 psi
annealed
CMW® ELKONIUM 42 palladium based alloy
Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting poi..
Tensile Strength, Ultimate 372 MPa
54000 psi
Ametek P409L P/M Stainless Steel, Sintered from 6.45 g/cc Green Density
P409L is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and ha..
Tensile Strength, Ultimate 372 MPa
54000 psi
Ametek P409L/409CB P/M Stainless Steel, Sintered from 6.45 g/cc Green Density
P409L/409CB is a ferritic, weldable grade of stainless steel high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and h..
Tensile Strength, Ultimate 372 MPa
54000 psi
AK Steel ZINCGRIP® GA Hot Dip Galvannealed Carbon Steel, Dent Resistant (DR 180)
Compared to DS Type B, DR steels have higher initial YS which contributes to increased strength after forming.Information provided by AK Steel
Tensile Strength, Ultimate 372 MPa
54000 psi
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Bake Hardenable (BH 180)
Information provided by AK Steel
Tensile Strength, Ultimate 372 MPa
54000 psi
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Bake Hardenable (BH 210)
Information provided by AK Steel
Tensile Strength, Ultimate 372 MPa
54000 psi
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Bake Hardenable (BH 250)
Information provided by AK Steel
Tensile Strength, Ultimate 372 MPa
54000 psi
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Dent Resistant (DR 180)
Information provided by AK Steel
Tensile Strength, Ultimate 372 MPa
54000 psi
AK Steel ZINCGRIP® Hot Dip Galvanized Carbon Steel, Dent Resistant (DR 210)
Information provided by AK Steel
Tensile Strength, Ultimate 372 MPa

@Temperature 760 °C
54000 psi

@Temperature 1400 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..