Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3500 MPa | 508000 psi | |
China Tungsten YG13X Tungsten Carbide Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 3500 MPa | 508000 psi | |
China Tungsten YG8X Tungsten Carbide Information provided by China Tungsten |