Polymer Property : Tensile Strength, Ultimate = 3.79 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 3.79 - 4.48 MPa
550 - 650 psi
Sika Industry SikaFlex 252 One Part Polyurethane Adhesive
Sika 252 SikaFlex One Part Polyurethane AdhesiveA high viscous, high strength adhesive, this product can replace rivets, screws, welds, and other mechanical fasteners. Seals and bonds in one step. 4..
Tensile Strength, Ultimate 3.79 MPa
550 psi
Dow Corning HS II BASE & 10:1, COLORED CATALYST
High strength silicone mold making rubber, suited for the detailed reproduction of fiines, art objects and similar items and better suited for thin section cure. HS II Base with HS II 10:1 Colored C..
Tensile Strength, Ultimate 3.79 MPa
550 psi
Dow Corning HS II BASE & SPRAYABLE COLORED CATALYST
High strength silicone mold making rubber, suited for the reproduction of robotic skins, tooling and immovable objects due to its thixotropic characteristics. HS II Base with HS Sprayable Catalyst C..
Tensile Strength, Ultimate 3.79 MPa
550 psi
Dow Corning SILASTIC® HV 1666/65 GRAY SILICONE RUBBER
65 Durometer, gray, peroxide cure, high voltage grade Silicone Rubber Compound for manufacturing High Voltage insulators weather shed insulators or surge arrestors. Superior wet electrical propertie..
Tensile Strength, Ultimate 3.79 MPa
550 psi
Dow Corning SILASTIC® L RTV SILICONE RUBBER BASE & CURING AGENT
Low durometer silicone mold making rubber recommended for use with rigid polyurethanes and can be used with polyesters and epoxies.Information provided by Dow Corning
Tensile Strength, Ultimate 3.79 MPa
550 psi
Loctite® Nuva-Sil® 5084 Sealant
Silicon Light Cure Adhesives and Gasketing and Wire TackersLoctite® innovative gasketing products offer precise, reliable sealing of electronic enclosures, protecting them from environmental hazard..