Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 3.45 MPa | >= 500 psi | ASTM D412 |
Multibase Multi-Flex® TPE A 6900 LC BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 3.45 MPa | 500 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tensile Strength, Ultimate | 3.45 MPa | 500 psi | |
Loctite® Ultra Grey® 5999 Flange Sealant Silicone GasketingLoctite® Silicone Gasketing materials include unique products with excellent resistance, formulations for high operating temperatures, and UV-curing formulations for cure-in-place.. |
|||
Tensile Strength, Ultimate | 3.45 MPa | 500 psi | |
Dymax 910 Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 910 Strain Relief, Wire and Parts Tacking AdhesiveFlexible, good adhesion and mechanical removable Cure Type: UV |
|||
Tensile Strength, Ultimate | 3.45 MPa | 500 psi | |
Dymax 952 Potting and Encapsulation Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 952 Potting and Encapsulation AdhesiveFast curing, high strength, flexible, excellent moisture resistance. Cure Typ.. |
|||
Tensile Strength, Ultimate | 3.45 MPa | 500 psi | Bond strength to metal |
Dymax Light Weld® 425 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Tensile Strength, Ultimate | >= 3.45 MPa | >= 500 psi | ASTM C297 |
Touchstone CFOAM® 25 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |
|||
Tensile Strength, Ultimate | 3.45 MPa | 500 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9201-75 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tensile Strength, Ultimate | 3.45 - 165 MPa | 500 - 23900 psi | Average value: 95.5 MPa Grade Count:92 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |