Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Pacific Sintered Materials F-241-T Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE V, CLASS AAll information provided by Pac.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Pacific Sintered Materials FCC-221-P Copper Steel Powdered Metal Applications:Medium strength mechanical componentsEquivalent MPIF Specification: FC-0205-35All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Pacific Sintered Materials FN-251-S Invar Powdered Metal Coefficient of thermal expansion equal to glass.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Pacific Sintered Materials SS-316-RH 316L Stainless Steel Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RH Powdered Metal Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Meehanite CC Corrosion Resisting Cast Iron Type CC is a general utility material providing good corrosive resistance. It can be used for slightly acid solutions, alkali solutions at temperatures up to 150 °F and concentrated sulfuric aci.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Meehanite HR Heat Resisting Cast Iron Type HR is a strong, dense iron of high rigidity and excellent resistance to scaling under most conditions. It possesses good load carrying ability. Recommended for service conditions without ther.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
MTI ThermoStran® PA66-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Williams Advanced Alloys WS280B Solder (Au80/Sn20) All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Williams Advanced Alloys WS305 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Tensile Strength, Ultimate | >= 276 MPa | >= 40000 psi | |
Alcoa Toolrite 2011®-T4 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Tensile Strength, Ultimate | 276 - 310 MPa | 40000 - 45000 psi | |
Eagle Brass 151 ZHC® COPPER, 1/4 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Ultimate | 276 - 434 MPa | 40000 - 63000 psi | |
Eagle Brass 194 HSM® Copper, Annealed High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Ultimate | 276 - 345 MPa | 40000 - 50000 psi | |
Eagle Brass 220 Commercial Bronze, 1/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | Annealed |
CMW® D154F Pre-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3 For electrical contacts; resistant to welding and high surge currents.Information provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | Annealed |
CMW® D355F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | Annealed |
CMW® D55F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781, Table 3 For electrical contacts; resistant to welding and high surge currentsInformation provided by CMW Inc. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | Typical |
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
Dura-Bar G2A Continuously Cast Gray Iron Bar Stock ASTM A48 Dura-Bar G2A has Type D graphite in a predominantly pearlitic matrix. The fine graphite structure allows excellent surface finish and is normally used in permanent mold applications requiring optima.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | annealed |
CMW® ELKONIUM 18 silver, copper, cadmium alloy The alloying of silver with cadmium produces materials with good arc extinction, good corrosion resistance and low contact resistance characteristics and provides them with good switching capability.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | cold worked |
CMW® ELKONIUM 28 Silver Alloy ELKONIUM® 28, a silver-manganese alloy, was developed by CMW specifically for the control of the transfer of contact material in low voltage DC applications. It is used as a positive contact operat.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | annealed |
CMW® ELKONIUM 72 gold based alloy Pure gold has complete resistance to atmospheric tarnish and oxidation. It does not contribute to polymer formations like platinum and palladium alloys. Wrought gold metal is very soft and prone to .. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
AIM CASTIN Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
AIM SAC305 Lead-Free Solder for Photonic Packaging This alloy falls under the JEIDA recommendation for lead-free soldering. When used in wave soldering, AIM’s SAC305 bar solder offers far superior fluidity as compared to other alloys and makes of b.. |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
PSM Industries Pacific Sintered Metals Invar FN-251-S Powdered Metal Coefficient of thermal expansion equal to glassInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Tensile Strength, Ultimate | 276 MPa | 40000 psi | |
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type V, Class AInformation Provided by Pacific Sintered Metals, a di.. |