Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 265 MPa @Temperature 980 °C |
38400 psi @Temperature 1800 °F |
|
Haynes 188 alloy, hot rolled and 1175°C solution annealed plate Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Ultimate | 265 MPa @Temperature 870 °C |
38400 psi @Temperature 1600 °F |
|
Haynes Hastelloy® W alloy, shielded metal arc welds, as-welded Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica.. |