Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2.83 MPa | 410 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9111-35W222 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for use in difficult injection molding applications and those requiring good flex.. |
|||
Tensile Strength, Ultimate | 2.83 - 14.0 MPa | 410 - 2030 psi | Average value: 10.7 MPa Grade Count:15 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an.. |