Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO 1047-3000 The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO 1047-3000 COMPOUND The burn rate is 0.53 in/min; ASTM FM VSS 302.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | |
Freudenberg Simrit V75WH Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | 500mm/min; ASTM D638 |
LG Chemical SEETEC BC500 LDPE Good Processability and Good electrical properties. Main Application: Cable insulationCAS No. 9002-88-4Information provided by LG Chemical |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | 500mm/min; ASTM D638 |
LG Chemical SEETEC BF415 LDPE Characteristics: Good Processability and Excellent Optical Properties Applications: Masking filmCAS No. 9002-88-4Information provided by LG Chemical |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | 500mm/min; ASTM D638 |
LG Chemical SEETEC BF500 LDPE Characteristics: Good Processability and Good Optical Properties Additives: Antiblocking Agent, Slip AgentApplications: Industrial Film & Food PackageCAS No. 9002-88-4Information provided by LG Chem.. |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | 500mm/min; ASTM D638 |
LG Chemical SEETEC BS500 LDPE Characteristics: Good Processability and Good cell uniformity& stability Additives: Antioxidant, Antiblocking agent, Slip AgentApplications: Foam sheetInformation provided by LG Chemical |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | |
Dow Primacor® 3150 Ethylene Acrylic Acid (EAA) PRIMACOR® 3150 polymer containing 3% comonomer is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion to metallic, pap.. |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | |
Dow Primacor® 4311 Ethylene Acrylic Acid (EAA) PRIMACOR® 4311 polymer containing 3% comonomer 3 is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion to metallic, p.. |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1790 psi | ASTM D638 |
Colorite Polymers Elastichem 5511TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Tensile Strength, Ultimate | 12.3 MPa | 1780 psi | ASTM D638 |
Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5302FR is a non-halogen, flame retardant grade.Information provided by Samyang. |