Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 10.8 MPa | 1560 psi | post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4550 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 10.8 - 20.6 MPa | 1560 - 2990 psi | ASTM D638 |
Polikim EFALON® K-25 PTFE, 25% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
Tensile Strength, Ultimate | 10.8 - 15.7 MPa | 1560 - 2280 psi | ASTM D638 |
Polikim EFALON® K-35 PTFE, 35% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1570 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1570 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1570 psi | ISO 37 |
Kuraray SEPTON® S2063 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1570 psi | |
Kuraray SEPTON® S64 Soft Compound Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre.. |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1560 psi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 180 FT EB Thermoplastic Vulcanizate Neoplast 180 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1570 psi | |
Dow LDPE 640IM Low Density Polyethylene DOW LDPE 640IM resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate stiffness for general purpose, and cap.. |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1570 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2090 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1570 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 10.8 MPa | 1570 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2090 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |