Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 9.04 - 583 J | 6.67 - 430 ft-lb | Average value: 63.3 J Grade Count:21 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Falling Dart Impact | 9.04 J | 6.67 ft-lb | ASTM D3029 |
Total 965E Polystyrene
(discontinued **) Polystyrene 965E is a high-impact polystyrene. The extruder will see that 965E produces sheet with a dull matte finish and superior wetting tension to meet the printers needs.965E is specially desig.. |
|||
Falling Dart Impact | 9.04 J | 6.67 ft-lb | 73°F; ASTM D3029 |
Spartech SP-2010 HIPS Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 9.04 J | 6.67 ft-lb | 73°F; ASTM D3029 |
Spartech SP-2050 Glossy HIPS Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |