Mechanical Properties Metric English Comments
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1301V-7 Polycarbonate Resin
Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1302-07 Polycarbonate Resin
Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin
Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1303-07 Polycarbonate Resin
Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203 m/min; ASTM D1822
Styron CALIBREâ„¢ 201-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203 m/min; ASTM D1822
Styron CALIBREâ„¢ 301-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 90.0 J
66.4 ft-lb
8000 ipm; ASTM D3763
Styron EMERGEâ„¢ 4310-6 Polycarbonate
EMERGEâ„¢ PC 4310-6 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Equ..
Dart Drop, Total Energy 90.0 J
66.4 ft-lb
8000 ipm; ASTM D3763
Styron CALIBREâ„¢ 2060-6 Polycarbonate
CALIBREâ„¢ 2060-6 resin is designed for medical applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity..
Dart Drop, Total Energy 90.0 J
66.4 ft-lb
8000 ipm; ASTM D3763
Styron CALIBREâ„¢ 2061-6 Polycarbonate
CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and ..
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203 m/min; ASTM D1822
Styron CALIBREâ„¢ 302-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203 m/min; ASTM D1822
Styron CALIBREâ„¢ 303-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Dart Drop, Total Energy 90.0 J
66.4 ft-lb
8000 ipm; ASTM D3763
Styron EMERGEâ„¢ 4330-6 Polycarbonate
EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information ..
Dart Drop, Total Energy 90.0 J

@Thickness 3.20 mm
66.4 ft-lb

@Thickness 0.126 in
203m/min; ASTM D3763
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin
Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..