Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EX1332T PC Lexan* EX1332T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and is UV stabilized. It is availab.. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EX7631T PC EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion. |
|||
Dart Drop, Total Energy | 72.0 J | 53.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Lexan® LUX1814N PC |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® ML7664 PC Copolymer (Asia Pacific) Lexan* ML7664 polycarbonate (PC) siloxane resin, is a product targeting (profile) extrusion applications requiring extreme low temperature ductility. Lexan* ML7664 resin is a non-FR product availabl.. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT4143T PC Copolymer (Asia Pacific) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Asia Pacific) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Dart Drop, Total Energy | 72.0 - 169 J | 53.1 - 125 ft-lb | Average value: 90.1 J Grade Count:19 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East) XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1300-22 Polycarbonate Resin Description: LUPOY PC 1300-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1201-22 Polycarbonate Resin Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1201HP-22 Polycarbonate Resin Description: LUPOY PC 1201HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Dart Drop, Total Energy | 72.0 J | 53.1 ft-lb | 8000 ipm; ASTM D3763 |
Styron CALIBREâ„¢ 2061-22 Polycarbonate CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Dart Drop, Total Energy | 72.0 J | 53.1 ft-lb | 8000 ipm; ASTM D3763 |
Styron EMERGEâ„¢ 4310-22 Polycarbonate EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn.. |
|||
Dart Drop, Total Energy | 72.0 J | 53.1 ft-lb | 8000 ipm; ASTM D3763 |
Styron EMERGEâ„¢ 4330-22 Polycarbonate EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec.. |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 301 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 72.0 J @Thickness 3.20 mm |
53.1 ft-lb @Thickness 0.126 in |
203 m/min; ASTM D1822 |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Dart Drop, Total Energy | 72.0 J @Temperature 23.0 °C |
53.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |